The following are some images of metal experienced Chloride Stress Corrosion Cracking.
Inter granular SCC of an Inconel heat exchanger tube
Trans granular SCC of 316 stainless steel chemical processing piping system
CSCC occured on insulated vessel
CSCC occured on insulated vessel

CSCC occured on Condenser tube
CSCC on pipe
Inter granular SCC of a pipe